Layering stacks of scrap glass to get fused pieces to cut as multi color leaves or decorations for other pieces. I fused this with Bullseye Basic Fuse Firing schedule with slight alteration. Instead of 1490 degree processing temperature, i went to 1475 degrees instead. All else stayed the same.
400 dph........................................1225 degrees..................................hold 30 min
600 dph........................................1475 degrees..................................hold 10 min
FULL..............................................900 degrees..................................hold 1 hour
100 dph..........................................700 degrees...................................hold 0 min
FULL..............................................70 degrees.....................................OFF