I am at some sort of an impasse, not knowing which way to go, with so many choices. And for some of these choice I go halfway and then don't finish. Is this my ADHD, am I so unable to finish tasks? Yes, that partially seems to be the case. For example, I have done several pot and screen melts and I now have a wet tile saw, but I have not completed a full piece yet that incorporates a piece of the screen and pot melt. I did do one, incorporating that with black glass and that somewhat turned me off; the black glass was a little too extreme for my taste so perhaps that was the reason. In order to incorporate a piece of screen melt into a larger piece, you need to have the right color around, and I did not have the right color around. To get that color you have to be able to recognize it in a catalog and order it or go all the way to Manchester, and bring your chunk with you and match it. Also, most of the screen melts come out thicker than 1/4 " and so in order to correctly put it in a piece I would probably have to layer 2 1/2 to 3 pieces of glass. I now know that I could fire polish the piece and then it would flatten to 1/4" inch, although, in some cases this fire polishing causes devitrification. The only way around that is to sand blast it which I cannot do, not having the machine, or cover it with a thin layer of fine clear frit and fuse it again. If that works, I would still have to incorporate that into another piece, fuse that piece and then slump it, meaning two more firings. I don't know, I haven't done that yet, but will it devitrify after all those firings; would the glass even survive all those firings? That would make 4 total firings. And it is difficult to cut the outside piece correctly, making sure that everything fits and is in line. So what should I do, I have one piece from a screen melt that has some devitrification on it and I dont want to do anything with it.
I have also been cutting curvy squiggles in glass and found that pretty hard to do but I did do some and are not quite determined what to do with that, so now for both I am going to put them aside. I originally thought I could cover the squiggles with some decorative stuff and hang them in a screen melt. But that is problematic, how should I hang them with bails, or drill holes, and drilling holes takes some work. My drill does not work very fast and I am not so committed to that piece yet, so for this also I have to set it aside and think more about it.
It came to me to try out pocket vases. I could use my clear glass, which I have quite a lot of, but this will take a lot. I will have to open the kiln while it is draping and watch the progress. But i feel like it is worth a try and I also seem to like to try new things. Okay, so first I will put away all the other things I have been working on and remain unfinished. I have a lot of those kind of things and I want to finish things in the future. Then I will gather materials for the pocket vases. Here we go. Pocket vases seem to be more complicated than they appear. When the top piece of glass drapes over the fiber paper what will happen? If I want to include or create a design in the top piece of glass should i do that first. Well yes I should and then cut it into 2 pieces for a pocket vase. Also is the firing schedule I am using for this pocket vase going to work. I used the following firing schedule:
300 dph............................1025 degrees .......................................hold 20 mins.
300 dph.............................1245 degrees ......................................hold 15 mins
full......................................900 degrees ......................................hold 1 hour
100 dph..............................700 degrees........................................hold 2 hours
off
Well now I am going to look at Bullseye tip sheet on part sheets and making some on clear glass that I think will look nice in a pocket vase.
Carefully observed decisions and firing instructions for creating with glass. Thoughts on color, placement and reactions achieved through the glass work.
Sunday, March 20, 2016
Tuesday, March 8, 2016
This is the mold. Actually this is not the exact mold, this is the exact mold
It is flatter than the one above
It is flatter than the one above. I prefired 2 pieces of blank glass into an 8 inch circle, then I covered the center of the mold with black powder. I layered over the black power red fine frit which I enclosed in a circle of green frit. I placed the prefired panel over it and are currently firing it at the following schedule
275 dph............................1225 degrees...........................hold 1 hour
300dph..............................1330 degrees..........................hold 10 mins
300 dph..............................1465 degrees.........................hold 5 mins
full......................................900 degrees...........................hold 1 hour
Will the piece take the outside shape of the mold or did I have to precut that. I think I already proved to myself that the slump stage would be successful in fixing the outer shape but I am looking at it again for this in what is a complex or multi pointed shape. I hope it does take the shape. I filled the center part of the sunflower but in the next try I will use different colors and from this time I should know if the amount of frit that I used is correct or not.
It did not take the shape of the outside edges. some of the ends raised a bit and another broke off. I have to understand slumping molds better.
Irid glass
Irid clear fired face down and capped with royal blue.
Sunday, February 28, 2016
Small soap dish slump mold
Slump firing schedule:
300dph................................1250 degrees..............................hold 10 min
Full........................................900 degrees..............................hold 1 hour
100dph...................................700 degrees..............................off
Uneven edges, it is hard to cut both layers exactly the same.
So I tried another one with two layers of glass: one layer of 3mm clear glass, capped with thin 2mm green glass. I fused a stenciled design on the top of the piece of a yellow flower with black center and bright green stalks. I am currently fusing that piece with the following schedule, hoping that the ripples, slight though they are at the edges, will show up. So in order to achieve that I used the following firing schedule:
300dph...............................................1150 degrees.......................hold 10 mins
300dph................................................1220 degrees......................hold 15 mins
Full........................................................900 degrees......................hold 1 hour
100dph...................................................700 degrees.....................off
Hopefully this will pick up the edges in the mold, ever so slight but still nice. I still have not been able to reproduce the effect in the picture below. Will be able to extrapolate to other difficult slumping molds what I have to do to pick up all that they have and I get to learn a lot as I go on.
I am going to go back to making some unusual frit combinations and filling the mold with that. The stencil worked okay. In future tries I will work harder to get the design sharper, more precise, fill in spaces on stencil with more accuracy.
I like the one I previously made with clear frit mixed with other colors and the frit is not fine, it is at least medium so I can see little balls in the "cast leaf". Although the mold is in the shape of a leaf, it is also a soap dish so it is plenty deep and not a delicate cast glass piece. But I am trying to make it that way and fired it as a thin cast piece using the following schedule:
300 dph......................................1375 - 1400 degrees.....................hold 10 mins
I used 1375 degrees processing temperature, because it is good to fire it low at least to begin with.
Full...............................................900 degrees.............................hold 30 mins
Off

Thursday, February 18, 2016
Net leaf vein mold. Delphi glass recommends following firing schedule:300 dph...................................1360 degrees......................hold 20 mins
300 dph....................................1455 degrees.....................hold 5 mins
full...........................................900 degrees.......................hold 1 hour
100 dph.....................................700 degrees.............................off and then slump recommended firing is:
350dph......................................1100 degrees..............................10 mins
350 dph......................................1250 degrees..............................hold 15 mins
Full.............................................900 degrees................................hold 1hour
100 dph.......................................700 degrees...............................off
Saturday, December 12, 2015
Snowflakes and Stars christmas ornaments
snowflakes, stars and more stars. All of these that have been fired have been done so at tack fuse level. Now I am full fusing them to see which way I like it better. The full fuse schedule came from Deans Blog who also had a pattern for a snowflake with 1/4 inch strips of glass delicately place all around. This is how he says he fired it.:
500 dph.............................300 degrees....................................hold 5 mins
800 dph.............................1465 degrees..................................hold 5 mins
Full.......................................900 degrees.................................hold 30 mins
175 dph.................................800 degrees.................................hold 10 mins
Right now the most important thing is to see which looks better the tack fused or the full fused or whether I should have both. I also have come up with an idea to use the 1/4 inch strips and place the 1" colored squares on them to decorate them in a star. snowflake like pattern So right now I am full fusing this one and we shall see.
The tack fuse schedule that I used is as follows:
400 dph..................................1000 degrees........................hold 10 mins
600 dph...................................1360 degrees.......................hold 10 mins
Full ...........................................900 degrees.......................hold 30 mins
100 dph.....................................700 degrees........................off
So it is better to pick a firing schedule some where in between tack and full fuse
This tack fuse schedule hardly does anything. The sides do not pucker but the different pieces do stick to each other. I think if I determine that I still like the tack fuse best then I should make it fire higher and longer to get it to have some additional effects.
The full fuse looked awful. Perhaps because of the kind of glass that I used or even the placement of the glass but tack fused it looks better. this time I had two projects prepared, one a snowflake that needs full fusing and the other the star that I believe looks better tack fused. Before thinking I put both of them in there together and did not want to remove one, so decided to use a processing temperature that might be a good compromise between the two. So I am firing it to 1410 and holding only 5 minutes. Lets see if that lower temperature does not harm the full fusing of the snowflake and does not affect the good look of the tack fused star. I finally tried a little more heat and I liked the effect there. In this project I am alligning the points of the squares to the post to which they are attached instead of aligning them up and down and am firing them with the following schedule. I used this previously and I like how it came out but in this trial I am going to use the 1420 degrees as the processing temperature but I am only going to hold it for 5 minutes. It will go as follows:
400 dph....................1000 degrees.....................................hold 10 mins
600 dph.....................1420 degrees....................................hold 5 mins
Full.............................900 degrees.....................................hold 30 mins
100 dph.......................700 degrees..........................................off
so that, above, is the best firing schedu
Thursday, November 19, 2015
Christmas stocking
300 dph............................1250 degrees.....................hold 10 mins
Full...................................1420 degrees.....................hold 10 mins
Full....................................900 degrees......................hold 30-60 mins
60 dph................................700 degrees...........................off
Full...................................1420 degrees.....................hold 10 mins
Full....................................900 degrees......................hold 30-60 mins
60 dph................................700 degrees...........................off
Sunday, November 1, 2015
KILN CARVING
I cannot add a picture of bullseye glass striker 1120-0030. It turns into a pretty yellow when fired. But I tried to make sure it is not part of a series of glass that
"This style is not suitable for kilncasting because it can opalize and/or
become incompatible when held at high temperatures for an extended
period. It may also opalize and/or become incompatible in instances
where processes exceed the parameters of the test for compatibility. Testing recommended when heatwork exceeds these parameters.has gold in it and thus needs a 2 hour hold when processing."
So at further thought I am not going to use this glass for my kiln carving project. I am going to wait to buy a light transparent glass from Stained Glass Express on Thursday. I am also going to buy some additional fiber paper.
Did my kiln carving pick up the marks I had drawn on the fiber paper, marks of veins in leaves; ever so slightly. I guess it will need a second layers of fiber paper. So may be I should try that: a big leaf, one cut out covered with a second cut out of veins and on a stem. And perhaps it would improve in glass other than white. Perhaps I will put this on a piece of green transparent glass. But first I cut out circles and within those cut out circles I have placed another circle. Want to see negative and positive and its effects on glass through kiln carving. Positive and negative. The one on bottom is two circles cut out, with a smaller circle in center; the one above is 2 layers of two circles. One is 1/8th inch and the other is 1/16th inch.
Subscribe to: